As I began to refine the maiden's face I discovered that this log was a little drier than usual and the wood was prone to splinter easily. When working around the mouth area I couldn't cut the lips without the wood flaking and chipping. I coated the area with some PEG 6000. Hopefully this will soak into the wood and help it stay together while being carved. The PEG (polyethylene glycol) will attract water from the atmosphere and keep the wood moist. It seemed to work on other problem carvings in the past.